9:91:913:913
Media Manager
Namespaces
Choose namespace
Media Files
Files in 12:123
- applications-of-fracture-mechanics.svg
- 2020/08/18 20:32
- 22.3 KB
- crack-opening-displacement.svg
- 2020/08/18 20:32
- 7.6 KB
- estimating-risks-with-fracture-mechanics.svg
- 2020/08/18 20:32
- 124.2 KB
- factors-causing-a-forced-feracture.svg
- 2020/08/18 20:32
- 215.1 KB
- forced-fracture-behavior-by-section-thickness.svg
- 2020/08/18 20:32
- 44 KB
- fracture-behavior-of-britte-materials.svg
- 2020/08/18 20:32
- 22 KB
- influences-on-fracture-toughness.svg
- 2020/08/18 20:32
- 18.5 KB
- overload-fractures-.svg
- 2020/08/18 20:32
- 18.4 KB
- stable-and-unstable-crack-growth.svg
- 2020/08/18 20:32
- 12.1 KB
- strength-of-ceramics.svg
- 2020/08/18 20:32
- 39.5 KB
- unstable-crack-mechanism.svg
- 2020/08/18 20:32
- 15.1 KB
File
- View
- History
- Date:
- 2021/07/05 12:32
- Filename:
- damage-symptoms-of-stress-corrosion-cracking.svg
- Size:
- 30KB
- References for:
- 16.2.2.7 Cracking during the Finishing Process